Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.76 GPa | 980 ksi | Tangent; ASTM D790 |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | Tangent; ASTM D790 |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | Tangent; ASTM D790 |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | Tangent; ASTM D790 |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
PolyOne Nymax™ MF 1200 A 40 HS Natural Polyamide 66 (Nylon 66) The Nymax® MF 1200 Series of mineral-reinforced nylon 6/6 compounds have been specifically engineered to provide an excellent balance of physical property performance, toughness, chemical resistanc.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
Niche Polymer PPHG40BK Homopolymer PP, 40% Glass Fiber Filled Information provided by Niche Polymer |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
Quadrant EPP Duratron® PAI T5030 Polyamide-imide, glass reinforced, extruded (ASTM Product Data Sheet) |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY DX08333 PC (Asia Pacific) LNP Lubriloy* DX08333 is an internally lubricated compound based on Lexan* Polycarbonate resin. Added features of this material include: ESD Safe, PTFE-free Wear & Friction solution and balanced mec.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFPPCC-40 40% Glass Reinforced Polypropylene Polifil® GFPPCC series compounds are homopolymer polypropylenes reinforced with chemically coupled glass fibers. These compounds offer superior strength and stiffness, improved elevated temperature.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | 8 lb Core, 6 hrs @ 220°F, Vacuum Bag |
Zyvex Performance Materials Aroply™ 250 Nano-Engineered Composite Film Adhesive Aroply™ 250 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported knitted nylon carrier. Cured adhe.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | |
BCC Products BC 6004 Epoxy Surface Coat BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thi.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | |
BCC Products BC 7009-1 Epoxy Casting BC 7009-1 is an iron filled, low-cost mass casting system. Thicknesses up to two inches in non-conductive molds, and four inches in conductive molds can be achieved without foaming or yielding exces.. |
|||
Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
PolyOne Edgetek® ATH-25GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |