BCC Products BC 6004 Epoxy Surface Coat

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 6004 Epoxy Surface Coat.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thickness of 1/8” or less on vertical surfaces or over sharp radii without sag or fear of run-off. BC 6004 features moderate heat resistance and tracing hardness.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 89

@Temperature 23.9 °C
89

@Temperature 75.0 °F
Tensile Strength, Ultimate 46.9 MPa
6800 psi
Flexural Strength 59.3 MPa
8600 psi
Flexural Modulus 6.76 GPa
980 ksi
Compressive Strength 95.1 MPa
13800 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.9 °C
174 °F
Processing Properties Metric English Comments
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
Pot Life 15 - 20 min

@Temperature 24.0 °C
15 - 20 min

@Temperature 75.2 °F
4 oz. mass
Descriptive Properties Value Comments
Mix Ratio 12:1 by weight, 7:1 by volume, resin/harder
Mixed Viscosity, Brookfield Thixotropic