| Category | Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Carbon + PTFE Filled |
| Manufacturer | Techmer ES |
| Trade Name | Electrafil® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | ASTM D792 |
| Water Absorption | 0.15 % | 0.15 % | 24 hrs. ASTM D570 |
| Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 96.5 MPa | 14000 psi | ASTM D638 |
| Elongation at Break | 2.5 % | 2.5 % | ASTM D638 |
| Flexural Yield Strength | 131 MPa | 19000 psi | ASTM D790 |
| Flexural Modulus | 6.76 GPa | 980 ksi | ASTM D790 |
| Izod Impact, Notched | 0.587 J/cm @Thickness 3.17 mm |
1.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Izod Impact, Unnotched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 148 °C | 298 °F | ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM C611 |
| Surface Resistance | 10000 ohm - 1e+05 | 10000 ohm - 1e+05 | ASTM D257 |