Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | Tangent; ASTM D790 |
RheTech Products GC30P200-01BG 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, General Purpose Black, Blow Molding Grade Applications: Load floorSeat backFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Nymax™ GF 600 A 14 Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Nylene® Vexel™ B12GF15 , 15% Glass Reinforced PBT Description: Vexel™ B12GF15 is a 15% glass fiber reinforced, general purpose PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeri.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Flexural Modulus | 4.48 - 17.2 GPa | 650 - 2500 ksi | Average value: 7.75 GPa Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Solvay Specialty Polymers Torlon® 4601 Polyamide-imide (PAI) Torlon® 4601 is a specialty wear-resistant grade of polyamide-imide (PAI). Most Torlon® PAI grades cannot be molded successfully in molds with undercuts. Torlon® 4601 has been formulated to.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF VF003 PA 66 (Asia Pacific) LNP* THERMOTUF* VF003 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Chase Plastics CP Pryme® N110GL (DAM) Nylon 6, 10% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Chase Plastics CP Pryme® N313GL (DAM) Nylon 6 (Utility Grade), 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Ensinger XP-151 Compression Molded PI Compound, 15% Graphite Filled, Premium Grade The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Edgetek® NL-10GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Asahi Kasei Thermofil N3-13FG-1626 13% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Lubri-Tech™ RA-15GF/13T Polyethersulfone, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 V0UL 94 (CTI Testing)PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |