Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS) Information provided by PolyOne |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Flexural Modulus | 20.0 GPa @Temperature 23.0 °C |
2900 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 6-7595 Polyamide 12, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Especially suitable at dynamic.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1105-7781/BK PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | |
Lehmann & Voss LUVOCOM® 1106-7227 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXS PA 66 (Asia Pacific) LNP* Thermocomp* RF00CSXS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | 0° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |
|||
Flexural Modulus | >= 20.0 GPa | >= 2900 ksi | IEC 1212-2 5.2 |
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-763 ABS - Flame Retardant F.R. High Heat Weather Resistant |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am.. |
|||
Flexural Modulus | 20.0 GPa | 2900 ksi | ASTM D790 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |