Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 757 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 128 MPa
18600 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 207 MPa
30000 psi
ASTM D790
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm
5.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 280 - 290 °C
536 - 554 °F
Deflection Temperature at 0.46 MPa (66 psi) 254 °C
489 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 299 - 310 °C
570 - 590 °F