Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.85 GPa | 413 ksi | |
Plastcom SLOVASTER® B1 GF 6/2 PBT reinforced with 6% glass fibre Features: PBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
NatureWorks® Ingeo™ 4032D Film Grade PLA NatureWorks® PLA (polylactide) polymer 4032D can be converted into a biaxially oriented film with use temperatures up to 300°F (150°C). This film has excellent optics, good machinability and exce.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® C50 PA66/6 Co-Polymer Description: NYLON 66/6 copolymerApplication: CompoundingInformation provided by NILIT. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® P36 Very High Flow Nylon 66 Description: Very high flowApplication: CompoundingInformation provided by NILIT. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® P40 Low Viscosity Nylon 66 Description: Low viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® P50 Standard Viscosity Nylon 66 Description: Standard viscosityApplication: CompoundingInformation provided by NILIT. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1005 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1005 Resin. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics EXTEM XH1005F TPI Resin (Europe-Africa-Middle East) High Heat Amorphous TPI Blend, Tg 267C, High Continuous Use Temperature (CUT). EFSA Food Contact Approved. Material is UL listed. This material is RoHS compliant and also halogen free according VDE/.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® P50FI Internally Lubricated Nylon 66 Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Nilit Polynil® P50L Externally Lubricated Nylon 66 Description: Polynil P50L is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips. It is also suited for monofilament extrusion.Key characteristics: Ex.. |
|||
Flexural Modulus | 2.85 GPa | 414 ksi | DIN 53452; ASTM D790 |
Kolon NOPLA® KE831 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Flexural Modulus | 2.85 GPa @Temperature 80.0 °C |
413 ksi @Temperature 176 °F |
2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl NH3060 PPE+HIPS NH3060 resin is a modified PPE + PS blend with an excellent balance of non-chlorinated non-brominated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific .. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ISO 178 |
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Chase Plastics CP Pryme® A100HF ABS Features: High FlowGeneral PurposeGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | ASTM D790 |
Tipco Tipcolene® FPT 20 - 20% Talc Reinforced Polypropylene Homopolymer Compound 20% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 2.85 GPa | 413 ksi | SAE J949 |
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |