Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® GHT3330 ABS (Asia Pacific) High heat grade of ABS used for interior automotive components.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9254 PC Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific) Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DBP32EI PC LNP* Lubricomp* DBP32EI is a compound based on Polycarbonate resin containing 15% PTFE/Silicone and 10% Glass Bead. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
LATI LASTIROL R-V2 Polystyrene (PS) (UL94 V-2)
(discontinued **) Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Flexural Modulus | 2.75 GPa | 398 ksi | DIN 53452; ASTM D790 |
Kolon KOPA® KN111 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Flexural Modulus | 2.75 GPa @Thickness 3.20 mm |
398 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP IBI16 PA 6/12 LNP LUBRICOMP* IBI16 is a compound based on Nylon 6/12 resin containing 30% Glass Bead, 2% Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KP003AXZ Acetal Homopoly (Asia Pacific) LNP* Lubricomp* KP003AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 LNP* LUBRICOMP* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific) LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp CI001 PS (Asia Pacific) LNP* Lubricomp* CI001 is a compound based on Polystyrene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C6303 PC+ABS LNP* Lubricomp* Cycoloy_C6303 compound is a Wear resistant (5% PTFE), flame retardant PC+ABS. High heat and good hydrolytic stability. UL listing from Japan and Pacific. |
|||
Flexural Modulus | 2.75 GPa | 399 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing 20% Glass Bead, 15% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retard.. |