Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 161J1-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 161J-4-DD Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | |
Plastcom SLOVALEN PC 19 GF 20 PP, 20% glass fibre, mod. of mech. properties FeaturesModified copolymer PP for iextrusion, chemically reinforced with 20% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied i.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS (Europe-Africa-Middle East) Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
PTS Trilac® TR558-CL ABS- Transparent ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | Molded; ASTM D790 |
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 .. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® F 6510 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
LG Chemical LUCEL VC-145 Antistatic POM, Unreinforced, Ultra High Flow, For VCR Reels LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1100A(W) PA6, Low Viscosity Feature: Injection Molding, PA6, Low ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 6.40 mm |
384 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
15 mm/min; ASTM D790 |
LG Chemical XR440 ABS, Low Emission High Heat ABS Feature: Injection Molding Grade, Low Emission High Heat ABSApplication: Automotives Interior housingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa @Thickness 3.20 mm |
384 ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific) NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON KX96321 POM LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 IM 3757 Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Copolymer, Impact Modified and LubricatedProcessing Method: Injection Mold.. |
|||
Flexural Modulus | 2.65 GPa | 385 ksi | ASTM D790 |
Techmer ES Plastiblend® TPX-HTN-000BB Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ASTM D790 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | Tangent; ASTM D790 |
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.65 GPa | 384 ksi | ISO 178 |
Polyplastics Duracon® HP25X Acetal Co-polymer (POM), High stiffness, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |