Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.43 GPa | 352 ksi | 13 mm/min; ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion LR620 white 1046 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® ML7682 PC Copolymer (Asia Pacific) Lexan ML7682 resin is a flame retardant polycarbonate blend featuring high flow, good processability, good impact, good heat resistance, and UV stability. It is of non-chlorine and non-bromine flame.. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 (Asia Pacific) LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON IS000XXL PA6.12 LNP* STAT-KON* IS000XXL is a compound based on Nylon 6/12 containing Stainless Steel Fibers. Added features of this material include: Food Contact Compliant Raw Materials, Metal Detectable, Electr.. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354P PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating performance, a good candidate for Laser Direct Structuring applications. |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | ASTM D790 |
Teknor Apex APEX® RS 9011A Polyvinyl Chloride, Rigid Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Stat-kon IS000LX PA6.12 LNP* Stat-Kon* IS000LX is a compound based on Nylon 6/12 containing Stainless Steel Fibers.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 1501E Description: Extrusion GradeInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 1502 Description: Injection Molding Grade, High GlossInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 7501 E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | ASTM D790, ISO 178 |
EPICHEM Epilon PC IX3000 Polycarbonate, High Impact Characteristics: high fluidity, high impact |
|||
Flexural Modulus | 2.43 GPa | 353 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA TW-18B2 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA TW-20 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | |
Abatron AboCast 50-6/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | ASTM D-790 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Flexural Modulus | 2.43 GPa @Thickness 19.0 mm |
352 ksi @Thickness 0.750 in |
ASTM D790 |
3A Composites Core Materials AIREX® PXw.420 Fiber-Reinforced Structural Foam Panel AIREX® PXw is a closed-cell, fiber reinforced polymer foam panel with a special formulation and very high mechanical properties. The sophisticated manufacturing process evenly distributes continuou.. |
|||
Flexural Modulus | 2.43 GPa | 352 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |