Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4000 - 6000 cP | 4000 - 6000 cP | 50-6 |
70 cP @Temperature 70.0 °C |
70 cP @Temperature 158 °F |
at 100/28 (50-6/50-17) pbw |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell M | 109 | 109 | |
Tensile Strength, Ultimate | 68.95 MPa | 10000 psi | |
Elongation at Break | 3.0 % | 3.0 % | |
Flexural Yield Strength | 105.28 MPa | 15270 psi | |
Flexural Modulus | 2.43 GPa | 352 ksi | |
Compressive Yield Strength | 118.25 MPa | 17151 psi | |
Compressive Modulus | 1.50 GPa | 217 ksi | |
Izod Impact, Notched | 0.235 J/cm | 0.440 ft-lb/in |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 157 °C | 315 °F | Deflection temperature; load unknown. |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.21e+16 ohm-cm | 1.21e+16 ohm-cm | |
Surface Resistance | >= 7.85e+15 ohm | >= 7.85e+15 ohm | |
Dielectric Constant | 3.6 @Frequency 1e+6 Hz |
3.6 @Frequency 1e+6 Hz |
|
4.01 @Frequency 1000 Hz |
4.01 @Frequency 1000 Hz |
||
4.07 @Frequency 60 Hz |
4.07 @Frequency 60 Hz |
||
Dissipation Factor | 0.0057 @Frequency 60 Hz |
0.0057 @Frequency 60 Hz |
|
0.015 @Frequency 1000 Hz |
0.015 @Frequency 1000 Hz |
||
0.34 @Frequency 1e+6 Hz |
0.34 @Frequency 1e+6 Hz |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 94.0 min @Temperature 70.0 °C |
94.0 min @Temperature 158 °F |
500 g |
Descriptive Properties | Value | Comments |
---|---|---|
Exotherm | 240°C | Peak |