Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
PolyOne LubriOne™ AT-000/05T Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Polymer Resources PPX-GP1 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Injection MoldingNotes: All physical, mechanical and thermal testing.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® OQ3820 PC (Asia Pacific) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | 0.05 in/min; 3-point; ASTM D790 |
Americas Styrenics STYRON™ A-TECH™ 1220 High-Impact Polystyrene Resin
(discontinued **) STYRON™ A-TECH™ 1220 advanced technology polystyrene resin is a high impact, high modulus resin for extrusion thermoforming applications. The improved durability of this resin allows potential do.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
M. Holland Company PC406UR Polycarbonate High impact resistanceGood mold releaseGood UV resistanceHigh viscosityApplications: AppliancesProtective coveringsDecorative displaysHousings |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Spartech Royalite R922 PC/ABS Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8005 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | 2.0 mm/min; ASTM D470 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 302V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity (for tinted/transparent colors), and is available in both tint.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Chase Plastics CP Pryme® A100 ABS Molding Resin Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Formosa Plastics Formolon® APW Compound APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ASA/PC TA-35 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Clariant PCSP0014 GREY Polycarbonate, Stainless Steel Fiber, EMI Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D-790 |
Axiall 9109J Clear Rigid PVC, Extrusion, Clear Georgia Gulf 9109J Clear is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer, which retards color change.Information provided by Georgia GulfGeo.. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D-790 |
Axiall 8132 Rigid PVC, Extrusion Georgia Gulf 8132 is a rigid PVC compound designed for applications where transparency is important. This product remains unchanged except for the coded name and was previously identified as 3132. .. |
|||
Flexural Modulus | 2.41 GPa | 350 ksi | ASTM D790 |
Aaron Industries AAROPRENE® AEPC 5000-3 Engineered Polycarbonate Resin Melt flow index may be specified. |
|||
Flexural Modulus | 2.41 - 2.55 GPa | 350 - 370 ksi | ASTM D790 |
Alcoa KAMA 4223 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 50”Silicone coatingCl.. |