Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolon® APW Compound

Category Polymer
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® APW Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
APW Powder Window Profile Compound Series The APW compounds have been designed for profile extrusion in window lineals, fencing and other outdoor weatherable markets. It exhibits excellent whiteness, surface and processing properties in a wide range of applications.Information provided by Formosa Plastics Corporation, USA
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.4 MPa
6150 psi
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Yield Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 10.7 J/cm

@Thickness 3.17 mm
20.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Dart Drop Total Energy 89.2 J/cm

@Temperature 0.000 °C
0.167 ft-lb/mil

@Temperature 32.0 °F
ASTM D4226
97.7 J/cm

@Temperature 23.0 °C
0.183 ft-lb/mil

@Temperature 73.4 °F
ASTM D4226
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Users viewing this material also viewed the following: