Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.28 GPa | 331 ksi | ASTM D790 |
PolyOne Novablend™ 9562 Polyvinyl Chloride Alloy (PVC Alloy) Custom MoldingInformation provided by PolyOne |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | Tangent; ASTM D790 |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC-UV4-[color]-1 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | ASTM D790 |
Covestro Apec® DP9-9331 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Flexural Modulus | 2.28 - 3.03 GPa | 331 - 439 ksi | Average value: 2.81 GPa Grade Count:12 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Global PC-1415-R General Purpose Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Global PC-FR2 UL Recognized 94V-2 Polycarbonate Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Spartech Royalite R60 PVC/Acrylic Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5500EX PBT+PC (Asia Pacific) Non-FR, non-UV PC/PBT blend for film extrusion application |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES HiFill® PC R GY143 Availability: North AmericaForms: PelletsFeatures: Low Smoke EmissionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Luriblend® HTN 05007 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Heat Resistance and LubricatedAppearance: BlackInformation provided by TP Composites, .. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D 790 |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Modulus | 2.28 GPa | 331 ksi | ASTM D790 |
Videolar 825 High Impact Polystyrene (HIPS) Injection molding gradeMedium melt flow and high glossGood balance between rigidity and impactFeatures: Excellent mechanical strengthExcellent temperature resistancehigh impactApplications: Toys, ap.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D-790 |
Axiall UV-6676 Rigid PVC, Molding Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | |
Abatron AboCast 8103-14 One-Component Epoxy AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
PlastxWorld CEVIAN®-V 400N ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Spartech Royalite R60-LS (R61) PVC/Acrylic Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |