Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall UV-6676 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall UV-6676 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as fence post caps, rain gutter parts, deck parts, etc.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D-785
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D-638
Tensile Modulus 2.21 GPa
320 ksi
ASTM D-638
Flexural Strength 65.5 MPa
9500 psi
ASTM D-790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D-790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
9.61 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
18.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 14.7 J

@Temperature 23.0 °C
10.8 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 65 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C
161.6 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
Flammability, UL94 5VA
5VA
Oxygen Index 35 %
35 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 230
Georgia Gulf Test
UL Weatherability Rating F(2)
UL-746C
Users viewing this material also viewed the following: