Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.28 GPa | 186 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Pro® 2520 XU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP FR 7C11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2907 HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss.Applications: Protective sports equipment, safety helmets, high impact custom molding.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2908C HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughnessApplications: Tote boxes, Beverage cratesAdditives: AntioxidantInformation provided by NOVA Chemicals. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP Mini-random homopolymer. Applications: BOPP film. Equivalent to Pro-fax® HL456JInformation provided by Phillips 66. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Edgetek® SY-15GB/000 Polystyrene (PS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extra high molecular weight polyethylene is tailored for large containers with exhibit outstanding impact and creep resistance, excellent ESCR, and e.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer COPYLENE™ CM200LN-02 is specially designed for injection molding applications where an excellent balance of stiffness/impact and good cycle times are required.Applications: Injection molding applic.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9025 , 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790A |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790B |
Ineos L12Z-01 Polypropylene Impact Copolymer Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provi.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent-Method; ASTM D790 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | secant; ASTM D790 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790-90 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | |
CMW® ELKONITE® 3W53 Heat Treatable Tungsten Copper material For resistance welding electrodes.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 3255 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers good impact strength, resistance to warpage, and stiffness. This product meets the Food and Drug Administration requ.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **) AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by .. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790A |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |