| Category | Metal , Metal Matrix Composite , Nonferrous Metal , Refractory Metal , Tungsten Alloy |
| Manufacturer | CMW Inc. |
| Trade Name | ELKONITE® |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | CMW® ELKONITE® 3W53 Heat Treatable Tungsten Copper material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 13.87 g/cc | 0.5011 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell B | 105 | 105 | |
| Flexural Modulus | 1.28 GPa | 186 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 85.0 W/m-K | 590 BTU-in/hr-ft²-°F | |
| Melting Point | 1080 - 3410 °C | 1980 - 6170 °F | |
| Solidus | 1080 °C | 1980 °F | |
| Liquidus | 3410 °C | 6170 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Copper, Cu | 30.86 % | 30.86 % | |
| Nickel, Ni | 0.88 % | 0.88 % | |
| Silicon, Si | 0.26 % | 0.26 % | |
| Tungsten, W | 68 % | 68 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.00000575 ohm-cm | 0.00000575 ohm-cm | (30% IACS) |