Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
NYCOA 7551 Copolymer Nylon Alloy resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc. |
|||
Flexural Modulus | >= 0.400 GPa | >= 58.0 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 0.400 GPa | >= 58.0 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | 2% Strain; ASTM D3350 |
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin Excellent ESCR, Excellent toughness, High strength, High flexibilityApplications: Pipes for pressure and non-pressure service from 12 mm to 100 mm, Potable water pipe and tubing, Underground sprinkl.. |
|||
Flexural Modulus | 0.400 - 3.00 GPa | 58.0 - 435 ksi | Average value: 2.19 GPa Grade Count:5 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Modulus | 0.400 - 16.8 GPa @Temperature -40.0 - 200 °C |
58.0 - 2440 ksi @Temperature -40.0 - 392 °F |
Average value: 5.22 GPa Grade Count:23 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flexural Modulus | 0.400 GPa @Temperature 100 °C |
58.0 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Flexural Modulus | 0.400 - 1.45 GPa | 58.0 - 210 ksi | Average value: 0.796 GPa Grade Count:35 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Flexural Modulus | 0.400 - 4.30 GPa @Temperature -40.0 - 80.0 °C |
58.0 - 624 ksi @Temperature -40.0 - 176 °F |
Average value: 2.14 GPa Grade Count:2 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP TH0300A PUR (Asia Pacific) LNP THERMOCOMP* TH0300A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade Applications:Drip irrigation pipeSmall potable water pipeInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178 |
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | DIN 53457/ISO 178 |
Borealis Borsoft™ SF203CF Soft Polypropylene Copolymer for Extrusion Coating Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
Borealis Borstar® LE8706 Natural Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8706 is a natural colorable linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar technology allows .. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM-D790 |
Polyram PlusTek RD120 Nylon 12, Injection Molding Polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178 |
Borealis Borsoft™ SA233CF High Impact Polypropylene Random Heterophasic Copolymer for Blown Film Borsoft SA233CF is a very soft random heterophasic copolymer, suitable for use on conventional blown film lines with air-coolingBorsoft SA233CF is especially suitable for soft packaging, hygienic fi.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ AK4504 TPO Compound Daplen AK4504 is a 30% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen AK4504 is a material with excellent impact/stiffness ratio. Thanks to its low th.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
Covestro Bayflex® 110-50 Polyurethane Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR6560 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ASTM D790 |
Ashley Polymers Ashlene® L930 Nylon 12 A plasticized Nylon 12 offering improved flexibility with superior moisture and chemical resistance. The natural color is slightly darker.Data provided by the manufacturer |
|||
Flexural Modulus | 0.400 GPa | 58.0 ksi | ISO 178 |
Borealis Borstar® LE8707 Black Bimodal LLDPE Jacketing Compound for Energy and Communication Cables Borstar® LE8707 is a black linear low density (LLD) jacketing compound, which is produced with the Borealis proprietary Borstar® bimodal process technology. Borstar® technology allows the manufa.. |