Material Notes:
Polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
DIN 53479
Water Absorption 1.5 %
1.5 %
DIN 53495
Linear Mold Shrinkage 0.0164 cm/cm
0.0164 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM-D638
Elongation at Break 300 %
300 %
ASTM-D638
Flexural Strength 20.0 MPa
2900 psi
ASTM D790
Flexural Modulus 0.400 GPa
58.0 ksi
ASTM-D790
Izod Impact, Notched 9.99 J/cm

@Temperature 23.0 °C
18.7 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 175 °C
347 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in