Material Notes:
Borsoft SF203CF is a new statistic-heterophasic propylene-ethylene copolymer suitable for coating applications. Its polymer structure permits perfect adhesion to certain products. According to the application, Borsoft SF203CF should be used preferably in blends with PP with high melt strength (HMS).Borsoft SF203CF is specially suitable for sealing layer, textile back sheet, breathable compounds, and soft coating.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133/DIN 5335
Mechanical Properties Metric English Comments
Tensile Strength, Yield 14.0 MPa
2030 psi
ISO 527-2
Elongation at Yield 15 %
15 %
ISO 527-2
Tensile Modulus 0.450 GPa
65.3 ksi
ISO 527-2
Flexural Modulus 0.400 GPa
58.0 ksi
DIN 53457/ISO 178
Charpy Impact, Notched 2.50 J/cm²
11.9 ft-lb/in²
ISO 179/1eA
0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 35.0 °C
95.0 °F
ISO 75 A
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
ISO 75 B