Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 23.0 J @Temperature -15.0 °C |
17.0 ft-lb @Temperature 5.00 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CB247G Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB247G high melt flow, 1,700 MPa flexural modulus, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of propert.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak, -30°C @ 2.2 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5521 PP SABIC® PPcompound 5521 is a mineral filled, impact modified polypropylene TPO. This material combines good flow with exterior automotive weathering stability. The general purpose black color prod.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Peak Energy; ASTM D3763 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Peak Energy; ASTM D3763 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Peak Energy; ASTM D3763 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HIPS3190 HIPS Complies with FDA Regulation 21 CFR 177.1640 for rubber modified polystyrene. HB rating from 0.062-0.125"" pending. Natural only. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -20.0 °C |
17.0 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak, -30°C @ 2.2 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 5310 PP SABIC® PPcompound 5310 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with exterior automotive weathering stability. The IMDS I.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
6.6 m/sec, Ductile; ASTM D3763 |
Styron INSPIRE™ TF7000 ES Natural Performance Polymer INSPIRE* TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications wher.. |