Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsApplications:Bakery Films, Coextr.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11D1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Strength and toughness, good sealing properties, suitable for narrow die gaps.Applications: Industrial packaging, heavy duty sacks.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11U4 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, easy processability.Applications: Bread bags, HDPE bottle sleeves, specialty blending.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Novapol® PF-Y821-D Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good blocking resistance.Applications: Bags-on-roll, produce bags, garment film, trash bags.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-103 LDPE Industrial Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer industrial film resin with excellent toughness. LD-103 has a low melt index which gives excellent impact strength and melt strength o.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-133 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ISO 527-3 |
Borealis Borsoft™ SD200CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD200CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation .. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | Film value |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | Film value |
Dow Elite® 5100 Linear Low Density Polyethylene 5100 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and puncture pro.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | 1%; ASTM D882 |
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | 1%; ASTM D882 |
Braskem LL 218 LLDPE Cast Film Extrusion Polyethylene Description: LL218 is a Linear Low Density Polyethylene, copolymer of butene-1, produced by Spherilene process. Developed for cast film extrusion. Films obtained with this product show a good proces.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | value @ 0.1 mm/mm-min Initial strain rate; ASTM D-882 |
Bapolene® 222F Polyethylene, Film Grade Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
Chevron Phillips 6335B LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip Version of 6335Characteristics: Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applications, Lo.. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer. |
|||
Secant Modulus, MD | 0.200 GPa | 29.0 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11M1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Co-extrusion.Data provided by the manufacturer. |