SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer SCG Chemicals Co.
Trade Name EL-Lene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SCG Chemicals EL-Leneâ„¢ L2020F Linear Low Density Polyethylene Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Characteristics:High output and elongationContains 1800 ppm slip agent and 1400 ppm antiblocking agentRecommended Applications:General purpose bag, cast film, small bag, merchandise bag, printed bagInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour

@Temperature 50.0 °C
>= 1000 hour

@Temperature 122 °F
F50, 25% Igepal; ASTM D1639
Thickness 38.0 microns
1.50 mil
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ASTM D882
Film Tensile Strength at Yield, TD 8.00 MPa
1160 psi
ASTM D882
Film Elongation at Break, MD 855 %
855 %
ASTM D882
Film Elongation at Break, TD 790 %
790 %
ASTM D882
Secant Modulus, MD 0.200 GPa
29.0 ksi
ASTM D882
Secant Modulus, TD 0.190 GPa
27.6 ksi
ASTM D882
Elmendorf Tear Strength, MD 4.92 g/micron
125 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 14.6 g/micron
370 g/mil
ASTM D1922
Dart Drop 2.40 g/micron
61.0 g/mil
ASTM D1709
Dart Drop Test 90.0 g
0.198 lb
ASTM D1709
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Film Tensile Strength at Break, TD 13.0 MPa
1890 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
ASTM D2117
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 13 %
13 %
ASTM D1003
Gloss 50 %
50 %
ASTM D2457