Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 6.21 MPa | 900 psi | Tensile; ASTM D1002 |
Protective Coating PC-Plumbing Epoxy Putty™ Hand Moldable, Multi-Purpose Epoxy Putty Stick Description: After Mixing, PC-Plumbing™ can be used to repair split and leaking pipes, tanks, drums, castings, ducts, valves and tools. It can be used wherever metal is missing, dented, broken, or .. |
|||
Shear Strength | 6.21 MPa @Treatment Temp. 65.0 °C, Time 7200 sec |
900 psi @Treatment Temp. 149 °F, Time 2.00 hour |
Lap |
Parker Chomerics CHO-BOND 584-29 Conductive Adhesive Two-component, highly conductive adhesive system that combines the good adhesive characteristics of epoxy with the superior conductivity of silver. In addition to being available in bulk form, the m.. |
|||
Shear Strength | >= 6.21 MPa | >= 900 psi | Tensile lap, Al to Al |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Shear Strength | >= 6.21 MPa | >= 900 psi | Tensile, Al to Al |
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
Shear Strength | >= 6.21 MPa | >= 900 psi | Bond, Al to Al |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Shear Strength | >= 6.21 MPa | >= 900 psi | Bond, Al to Al, after 30 days water immersion |
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat.. |
|||
Shear Strength | >= 6.21 MPa | >= 900 psi | Plate Shear, L Direction, min |
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Aluminum; ASTM D1002-64 |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, ABS; ASTM D1002-64 |
3M Scotch-Weld™ CA8 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, ABS; ASTM D1002-64 |
3M Scotch-Weld™ CA9 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting version of CA8 for wire tacking and coil terminating. Meets CID A-A-3097, Type II, C.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Wood, Fir |
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.Information provided b.. |
|||
Shear Strength | 6.21 MPa | 900 psi | ASTM D1002-72 |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |
|||
Shear Strength | 6.21 MPa @Temperature -29.0 °C |
900 psi @Temperature -20.2 °F |
Overlap, Green FRP, Adhesive Failure |
3M Scotch-Weld™ DP8005 Black Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, 304 Stainless Steel (1/32" thick), Adhesive Failure |
3M Scotch-Weld™ DP8010 Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polypropyl.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, 71°C/100% RH for 14 days, AF/CF |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Copper |
3M Scotch-Weld™ DP805 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP805 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact and durability .. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Acetone for 14 days, Cohesive Failure |
3M Scotch-Weld™ DP810NS Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Polycarbonate, Substrate Failure |
3M Scotch-Weld™ DP8405NS Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP8405NS is a high performance, two-part acrylic adhesives that offer excellent shear, peel and impact performance. These toughened adhesives provide improved adh.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, High Pressure Laminate, Substrate Failure |
3M Scotch-Weld™ Thick Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, ABS; ASTM D1002-64 |
3M Scotch-Weld™ CA40H Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity version of CA40 and better void filling capabilities.Information provided by 3M |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, ABS; ASTM D1002-64 |
3M Scotch-Weld™ CA7 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to metals, plastics, and rubbers.Information provided by 3.. |
|||
Shear Strength | 6.21 MPa @Temperature 82.0 °C, Time 14400 sec |
900 psi @Temperature 180 °F, Time 4.00 hour |
Aluminum, etched, Overlap, Adhesive Failure |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, Poplar, Substrate/Cohesive Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap, High Pressure Laminate, Substrate Failure |
3M Scotch-Weld™ Medium Instant Wood Adhesives and Surface Activator 3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap on Etched Aluminum, cured for 90 mins @ RT; ASTM D1002 |
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar.. |
|||
Shear Strength | 6.21 MPa | 900 psi | Overlap on Etched Aluminum, cured for 90 mins @ RT; ASTM D1002 |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |