| Category | Polymer , Thermoset , Epoxy , Epoxy Adhesive |
| Manufacturer | 3M |
| Trade Name | Scotch-Weld™ |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | 3M Scotch-Weld™ DP125 Gray Epoxy Adhesive.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Brookfield Viscosity | 35000 - 75000 cP | 35000 - 75000 cP | Base, RVF #7 spindle, 20 rpm @ 27°C |
| 45000 - 65000 cP | 45000 - 65000 cP | Accelerator, RVF #7 spindle, 20 rpm @ 27°C |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 70 | 70 | ASTM D2240 |
| Tensile Strength at Break | 22.8 MPa | 3310 psi | ASTM D882 |
| Elongation at Break | 125 % | 125 % | ASTM D882 |
| Shear Strength | 0.414 MPa | 60.0 psi | Overlap, Polypropylene |
| 1.72 MPa | 250 psi | Overlap, +3M Primer 3901 | |
| 2.76 MPa | 400 psi | Overlap, Glass, Borosilicate | |
| 3.59 MPa | 520 psi | Overlap, ABS | |
| 3.79 MPa | 550 psi | Overlap, Acrylic | |
| 5.17 MPa | 750 psi | Overlap, PVC | |
| 6.07 MPa | 880 psi | Overlap, Polycarbonate | |
| 6.21 MPa | 900 psi | Overlap, Wood, Fir | |
| 12.4 MPa | 1800 psi | Overlap, Fiberglass | |
| 13.1 MPa | 1900 psi | Overlap, Cold Rolled Steel | |
| 15.2 MPa | 2200 psi | Overlap, Sanded Aluminum | |
| 23.4 MPa | 3400 psi | Overlap, Etched Aluminum | |
| 2.76 MPa @Temperature 82.0 °C |
400 psi @Temperature 180 °F |
Overlap | |
| 3.10 MPa @Temperature 66.0 °C |
450 psi @Temperature 151 °F |
Overlap | |
| 4.83 MPa @Temperature 49.0 °C |
700 psi @Temperature 120 °F |
Overlap | |
| 23.4 MPa @Temperature -55.0 °C |
3400 psi @Temperature -67.0 °F |
Overlap | |
| 29.6 MPa @Temperature 21.0 °C |
4300 psi @Temperature 69.8 °F |
Overlap | |
| Peel Strength | 0.351 kN/m | 2.00 pli | 180° |
| 0.526 kN/m | 3.00 pli | 180° | |
| 0.526 kN/m | 3.00 pli | 180° | |
| 3.16 kN/m | 18.0 pli | 180° | |
| 6.14 kN/m | 35.0 pli | 180° |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 98.0 µm/m-°C @Temperature 5.00 - 20.0 °C |
54.4 µin/in-°F @Temperature 41.0 - 68.0 °F |
Below Tg |
| 187 µm/m-°C @Temperature 65.0 - 140 °C |
104 µin/in-°F @Temperature 149 - 284 °F |
Above Tg | |
| Thermal Conductivity | 0.151 W/m-K @Thickness 6.35 mm, Temperature 44.3 °C |
1.05 BTU-in/hr-ft²-°F @Thickness 0.250 in, Temperature 112 °F |
|
| Glass Transition Temp, Tg | 12.0 °C | 53.6 °F | Onset |
| 23.0 °C | 73.4 °F | Mid-Point |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | ASTM D257 |
| Dielectric Constant | 6.3 @Frequency 1000 Hz |
6.3 @Frequency 1000 Hz |
ASTM D150 |
| Dielectric Strength | 26.8 kV/mm @Thickness 0.762 mm |
680 kV/in @Thickness 0.0300 in |
ASTM D149 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 120 min | 2.00 hour | Tack-free |
| 150 min | 2.50 hour | Time to Handling Strength | |
| 420 min | 7.00 hour | Full |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Amber | Accelerator |
| Gray | Base | |
| Gray |