3M Scotch-Weld™ CA8 Instant Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ CA8 Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Slower setting than CA7 and excellent adhesion to metals, and plastics and rubbers. Meets CID A-A-3097, Type II, Class 2.Information provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 70 - 130 cP
70 - 130 cP
Mechanical Properties Metric English Comments
Shear Strength 0.241 MPa
35.0 psi
Overlap, Nitrile Rubber; ASTM D1002-64
0.379 MPa
55.0 psi
Overlap, Neoprene Rubber; ASTM D1002-64
6.21 MPa
900 psi
Overlap, ABS; ASTM D1002-64
6.89 MPa
1000 psi
Overlap, Rigid PVC; ASTM D1002-64
13.8 MPa
2000 psi
Overlap, Steel; ASTM D1002-64
14.5 MPa
2100 psi
Overlap, Aluminum; ASTM D1002-64
Peel Strength 0.351 - 0.701 kN/m
2.00 - 4.00 pli
T-Peel
Processing Properties Metric English Comments
Cure Time 0.083333 - 0.666666 min
0.0013889 - 0.0111111 hour
Descriptive Properties Value Comments
Appearance Clear