Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.9 MPa | 2300 psi | Tensile Shear Strength; ASTM D1002 |
Protective Coating PC-Clear™ Clear Liquid Epoxy PC-Clear™ is a completely clear liquid epoxy formulated to remain clear during and after its curing time. PC-Clear™ is very durable and flexible making it unlike many liquid epoxies. Uses include.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Cured, tensile, Al/Al |
Resin Technology Group EN 139-2 UV Gellable, Low Temperature Cure, One-Component Epoxy Adhesive EN 139-2 is a UV gellable, one-component epoxy based adhesive system designed to provide cure at temperatures as low as 80°C. This one-part adhesive gels to a tack-free, low strength polymer upon e.. |
|||
Shear Strength | 15.9 MPa @Temperature 316 °C |
2300 psi @Temperature 600 °F |
|
Greene Tweed Arlon® 1000 Polyketone Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Shear Strength | >= 15.9 MPa | >= 2300 psi | Bond, Al to Al |
Master Bond EP45HTAO Heat Resistant Epoxy for Structural Bonding Description: Master Bond Polymer Compound EP45HTAO is a two component thermally conductive epoxy compound for high performance structural bonding, and casting. It is suitable for applications where .. |
|||
Shear Strength | >= 15.9 MPa | >= 2300 psi | Tensile lap, Al/Al |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Shear Strength | >= 15.9 MPa | >= 2300 psi | Bond, Al to Al, after 30 days water immersion |
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding Description: Master Bond Polymer Adhesive SUPREME 45HTND is a two component epoxy adhesive featuring a balance of shear and peel strengths for high performance structural bonding suitable for applic.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Al/Al |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Etched Aluminum, 30 days tap water @ RT |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Abraded Aluminum, Initial |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Aluminum Oakite degrease |
3M Scotch-Weld™ DP460 NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Galvanized Aluminum (MEK/abrade/MEK), Adhesive Failure; ASTM D1002 |
3M Scotch-Weld™ DP920 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP920 is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive with a 20 minute work life. It exhibits excellent shear and peel strengths along with good i.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | |
3M Scotch-Weld™ DP601 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | |
3M Scotch-Weld™ DP601NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, 304 Stainless Steel (1/32" thick), Cohesive Failure |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Etched Al, Salt Spray at RT for 14 days |
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Steel; ASTM D1002-64 |
3M Scotch-Weld™ CA4 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M |
|||
Shear Strength | 15.9 MPa | 2300 psi | Overlap, Etched Aluminum, 30 days tap water @ RT |
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |