3M Scotch-Weld™ DP601NS Structural Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP601NS Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the components are automatically mixed and easily dispensed as a bubble-free self-leveling liquid.Information provided by 3M
Physical Properties Metric English Comments
Density 1.02 - 1.07 g/cc
0.0368 - 0.0387 lb/in³
Part B
1.14 - 1.19 g/cc
0.0412 - 0.0430 lb/in³
Part A
Brookfield Viscosity 1000 - 3000 cP
1000 - 3000 cP
Part A, CP #52 @ 100 rpm
1500 - 3000 cP
1500 - 3000 cP
Part B, CP #52 @ 100 rpm
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
after 1 hr cure
Shear Strength 15.9 MPa
2300 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.0 °C
-59.8 °F
Processing Properties Metric English Comments
Cure Time 2.00 min
0.0333 hour
Time to Handling Strength
60.0 min
1.00 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Yellowish
Part A
Medium-Gray
Opaque Black
Part B