Tensile Strength, Ultimate 6.14 - 175 MPa

@Temperature -40.0 - 160 °C
891 - 25400 psi

@Temperature -40.0 - 320 °F
Average value: 70.3 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Tensile Strength, Ultimate 6.14 - 175 MPa

@Strain 0.250 - 5.00 %
891 - 25400 psi

@Strain 0.250 - 5.00 %
Average value: 70.3 MPa Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Tensile Strength, Ultimate 65.5 - 175 MPa
9500 - 25400 psi
Average value: 114 MPa Grade Count:60
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Tensile Strength, Ultimate 76.0 - 175 MPa
11000 - 25400 psi
Average value: 132 MPa Grade Count:24
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max..
Tensile Strength, Ultimate 29.6 - 175 MPa
4300 - 25400 psi
Average value: 96.8 MPa Grade Count:156
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Tensile Strength, Ultimate 70.0 - 175 MPa
10200 - 25400 psi
Average value: 122 MPa Grade Count:71
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 40.0 - 175 MPa
5800 - 25400 psi
Average value: 105 MPa Grade Count:16
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu..
Copyright © lookpolymers.com All Rights Reserved