Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Plaskolite West Optix® CA-81 UVA UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | TM R050-36 |
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy EP950G Gray is an aluminum filled one part rubber modified epoxy designed for bonding metal and other structural material subject to stress at elevated temperature. It is a medium paste-like viscosi.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Plaskolite West Optix® CA-81 UVA-7 UV-Absorbing Acrylic Resin Special UV-absorption grade, extrusion and injection moldingApplications: A special UV-absorption acrylic resin for extrusion and injection molding. It is slightly lubricated for ease of processing.. |
|||
Tensile Strength, Ultimate | 65.5 - 175 MPa | 9500 - 25400 psi | Average value: 114 MPa Grade Count:60 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Tensile Strength, Ultimate | 65.5 - 138 MPa | 9500 - 20000 psi | Average value: 95.2 MPa Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC
(discontinued **) Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced
(discontinued **) Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM Data |
Styron CALIBRE™ 200 22 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM Data |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4630-10 Polycarbonate EMERGEâ„¢ PC 4630-10 advanced resin is formulated to supply both excellent ultraviolet stability and enhanced ignition resistance while maintaining excellent physical properties and processabilit.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4600-10 Polycarbonate EMERGEâ„¢ PC 4600-10 advanced resin is formulated to supply both clarity and enhanced ignition resistance while maintaining excellent physical properties. Applications: Information Technology E.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Abatron AboCast/AboCure 8109-3 Low viscosity, RT cure. Easy processing.Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
Abatron AboCast/AboCure 8109-8 All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mi.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ATSM D638 |
Ashley Polymers Ashlene® 520BU Nylon 66 A general purpose Nylon 66 resin, black, utility grade.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Applied Composites 8079 Modified Vinylester SMC Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Low Moisture and Absorption, Permeability, Paintable, Flexible Design Parameter, Thick Cross Sections, Hig.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
BCC Products BC 5008-2 General Purpose Epoxy System BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A.. |
|||
Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | ASTM D638 |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |