Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast/AboCure 8109-8

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast/AboCure
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast/AboCure 8109-8.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All-purpose, structural dielectric resin. High thermal and chemical resistance and RT cure.Processing: 100/12 ratio; Potlife: 45 min/20°C (68°F), 20 min/40°C (105°F), 10 min /60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°F), 10-20 min/100°C (212°F).Applications: Laminating, small volume potting and impregnating.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Water Absorption 0.30 - 0.40 %
0.30 - 0.40 %
(60x10X4 mm bar) after 10 days at 20°C (77°F)
0.60 - 1.0 %
0.60 - 1.0 %
(60x10X4 mm bar) after 1 hour at 100°C (212°F)
Viscosity 4500 - 6000 cP
4500 - 6000 cP
Vapor Pressure <= 0.0000133 bar

@Temperature 20.0 °C
<= 0.0100 torr

@Temperature 68.0 °F
AboCure
0.00133 bar

@Temperature 180 °C
1.00 torr

@Temperature 356 °F
AboCast
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.5 MPa
9500 psi
Modulus of Elasticity 3.447 GPa
500.0 ksi
Flexural Yield Strength 124.1 MPa
18000 psi
Compressive Yield Strength 124.1 MPa
18000 psi
Thermal Properties Metric English Comments
CTE, linear 65.0 - 70.0 µm/m-°C

@Temperature 20.0 °C
36.1 - 38.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.190 - 21.0 W/m-K
1.32 - 146 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.50e+16 ohm-cm
>= 1.50e+16 ohm-cm
Dielectric Constant 3.65 - 3.85

@Frequency 1e+6 Hz
3.65 - 3.85

@Frequency 1e+6 Hz
3.8 - 4.0

@Frequency 1000 Hz
3.8 - 4.0

@Frequency 1000 Hz
3.85 - 4.05

@Frequency 50 Hz
3.85 - 4.05

@Frequency 50 Hz
Dielectric Strength 15.7 - 19.7 kV/mm

@Thickness 3.17 mm
400 - 500 kV/in

@Thickness 0.125 in
Short time value
Dissipation Factor 0.0050 - 0.010

@Frequency 50 Hz
0.0050 - 0.010

@Frequency 50 Hz
0.010 - 0.015

@Frequency 1000 Hz
0.010 - 0.015

@Frequency 1000 Hz
0.025 - 0.030

@Frequency 1e+6 Hz
0.025 - 0.030

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Pot Life 10.0 min

@Temperature 60.0 °C
10.0 min

@Temperature 140 °F
20.0 min

@Temperature 40.0 °C
20.0 min

@Temperature 104 °F
45.0 min

@Temperature 20.0 °C
45.0 min

@Temperature 68.0 °F
Copyright © lookpolymers.com All Rights Reserved