Applied Composites 8079 Modified Vinylester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer Applied Composites Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 8079 Modified Vinylester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Industry Application: ElectricalProduct Application: Transmission ProductDistinct Features: Low Moisture and Absorption, Permeability, Paintable, Flexible Design Parameter, Thick Cross Sections, High FlowInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.78 g/cc
0.0643 lb/in³
ASTM D792
Water Absorption <= 0.10 %
<= 0.10 %
ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
Cold Part VS Cold Tool; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 55
55
ASTM D2583
Hardness, Rockwell M 111
111
ASTM D785
Tensile Strength, Ultimate 65.5 MPa
9500 psi
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D638
Flexural Strength 159 MPa
23000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
Tangent; ASTM D790
Compressive Strength 145 MPa
21000 psi
ASTM D695
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 0.30
0.30
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Flexural Load; ASTM D648
Flammability, UL94 V-0
V-0
1/4 in; UL746
V-0
V-0
1/8 in; UL746
V-0
V-0
1/16 in; UL746