| Category | Polymer , Thermoset , Epoxy |
| Manufacturer | Cotronics |
| Trade Name | Duralco™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Cotronics Duralco™ 4461 Electrically Resistant, Low Viscosity Epoxy Adhesive, Coating, and Sealant.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.10 g/cc | 0.0397 lb/in³ | |
| Moisture Absorption at Equilibrium | 0.15 % | 0.15 % | |
| Viscosity | 600 cP | 600 cP |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 80 | 80 | |
| Tensile Strength, Ultimate | 65.5 MPa | 9500 psi | |
| Elongation at Break | 5.0 % | 5.0 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 64.0 µm/m-°C @Temperature 20.0 °C |
35.6 µin/in-°F @Temperature 68.0 °F |
|
| Thermal Conductivity | 0.576 W/m-K | 4.00 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 260 °C | 500 °F | |
| Shrinkage | 0.80 % | 0.80 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm | |
| Dielectric Strength | 17.7 kV/mm | 450 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min @Temperature 121 °C |
0.500 hour @Temperature 250 °F |