Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638-61T |
Rotuba 880 Ethyl Cellulose Data provided by the manufacturer. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638 |
Huntsman Rexell® H2110 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: Good toughness, ESCR.Applications: Industrial and consumer pails, general purpose molding.Information provided by Huntsman Corporation |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638 |
LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityAppli.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638 |
LyondellBasell Astryn SD068-4 Polypropylene Copolymer, 40% Calcium Carbonate Key Features: fractional melt flow, high modulus, mineral-filled, blow molding and extrusion grade polypropylene copolymer, good melt strength, excellent processability, excellent impact and stiffne.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 389 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638 |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 392 Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ASTM D638 |
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 105 Non-Reinforced, Injection Molding Grade Sodium Ionomer DescriptionFormion® FI 105 is a non-reinforced, transparent, injection molding grade Sodium Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and .. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 391E Ionomer Information provided by A. Schulman. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 120E Non-Reinforced, Extrusion Grade Zinc Ionomer DescriptionFormion® FI 120E is a non-reinforced, transparent, extrusion grade Zinc Ionomer. It has been formulate for high durability, cut and puncture resistance, and low temperature ductility.Ap.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | ASTM D638/D412 |
Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | Dynamic tensile strength |
Channel Industries 1300 Barium Titanate Piezoelectric Navy IV typeModified barium titanates are widely used in transducers requiring moderate power level and receiving sensitivity. Special characteristics have made barium titanate a proven material for.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | at max load; ISO 527 |
A. Schulman FORMION™ FI 120 Non-Reinforced, Injection Molding Grade Zinc Ionomer DescriptionFormion® FI 120 is a non-reinforced, transparent, injection molding grade Zinc Ionomer. It has been formulated for high durability, scratch resistance, low temperature ductility, and lo.. |
|||
Tensile Strength, Ultimate | 21.0 - 48.0 MPa | 3050 - 6960 psi | Average value: 33.2 MPa Grade Count:11 |
Overview of materials for Ethyl Cellulose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ethyl Cellulose, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Tensile Strength, Ultimate | 21.0 MPa | 3050 psi | Cured 7 min at 177°C and Post Cured 16 hr at 232°C |
DuPont Performance Polymers GBL-200 Formulation
(discontinued **) FormulationViton® GBL-200 |