Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Astryn
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityApplications: small appliancesDescription: Astryn 73F5-1 medium high melt flow, 10% calcium carbonate-filled polypropylene copolymer has an excellent combination of strength, stiffness, impact resistance, colorability and processability.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792B
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 81
81
ASTM D785
Tensile Strength, Ultimate 21.0 MPa
3050 psi
ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 120 %
120 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
Tangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
ASTM D648
Users viewing this material also viewed the following: