Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 62.0 - 100 MPa | 8990 - 14500 psi | Average value: 93.8 MPa Grade Count:7 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM Data |
Dow Isoplast® 2520 Polyurethane (PUR-RT), Impact Modified
(discontinued **) ISOPLAST® 2520 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins specially designed for medical applications. Its outstanding properties include excel.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Custom Resins Duratel™ MF13 Acetal Copolymer
(discontinued **) Description: Duratel™ MF13 is a 13 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Cookson Group Plaskon® S-7LA Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low alpha emission molding compound designed for packaging stress-sensitive memory devices. It offers an alpha par.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Cookson Group Plaskon® S-7P Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | |
Cookson Group Plaskon® S-7S Epoxy Encapsulant
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A low stress, low viscosity epoxy encapsulant designed for packaging stress-sensitive semiconductor devices. It is specifically .. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | 5 mm/min; ISO 527 |
Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 1095 °C |
8990 psi @Temperature 2003 °F |
|
Haynes 214® alloy, hot rolled solution annealed plate 12.7 mm (1/2 in.) thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 22.0 °C |
8990 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Ineos ABS Lustran® SAN Sparkle Highest-Clarity |
|||
Tensile Strength, Ultimate | 62.0 MPa @Temperature 110 °C |
8990 psi @Temperature 230 °F |
ASTM D638 |
Saint-Gobain Meldin® 7001 Direct Formed Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2300 Phenolic, Granular, Compression Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Chem Polymer Chemlon 253 H Nylon 6, Impact Modified A medium viscosity impact modified, heat stabilized nylon 6 exhibiting improved toughness over general purpose nylon 6.Data provided by the manufacturer, Chem Polymer. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
A. Schulman ComAlloy Hiloy® 283 PPO Alloy, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled A mineral filled Nylon 66 providing superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® 735 Nylon 6 Economy grade, impact modified Nylon 6 for injection molding.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Custom Resins Duratel™ MF9 Acetal Copolymer
(discontinued **) Description: Duratel™ MF9 is a 9 melt flow, general purpose acetal copolymer. Information provided by Custom Resins. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ASTM D638 |
Covestro Apec® DP9-9353 High-Heat Polycarbonate, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ATSM D638 |
Ashley Polymers Ashlene® L935 Nylon 11 An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer |
|||
Tensile Strength, Ultimate | 62.0 - 83.0 MPa | 8990 - 12000 psi | Average value: 77.0 MPa Grade Count:10 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Tensile Strength, Ultimate | 62.0 MPa | 8990 psi | ISO 527-1, 2 |
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |