Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® HMG94MD ABS Superior flow, injection molding ABS for medical applications. Good impact. For thin-wall applications. Biocompatible (ISO10993). FDA compliant. Gamma & EtO sterilizable. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG94U ABS High flow, UV stabilized ABS molding grade |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32P PC LNP* LUBRICOMP* DFL32P is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Exceptional Processing. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi.. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXJ PC LNP* Lubricomp* DFL36XXJ is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare.. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC (Asia Pacific) LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature -15.0 °C |
15.5 ft-lb @Temperature 5.00 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CB259 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact r.. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 0.000 °C |
15.5 ft-lb @Temperature 32.0 °F |
Peak Energy, 135.0 m/min; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of .. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature -30.0 °C |
15.5 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB252 medium high melt flow, 1,200 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has very well balanced processability, rigidi.. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature -10.0 °C |
15.5 ft-lb @Temperature 14.0 °F |
Instrumented, Peak Energy, 405.0 m/min; ASTM D3763 |
LyondellBasell Hostacomâ„¢ CB280F Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CB280F high melt flow, 1,900 MPa flexural modulus, UV-stabilized, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, .. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11 LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | ASTM Test |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2F004 FP-E (EFTE) LNP* FP-EF-1004 is a fluoropolymer compound based on ETFE resin containing 20% Glass Fiber. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HFD4412 PC Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Europe-Africa-Middle East) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Dart Drop, Total Energy | 21.0 J @Temperature 23.0 °C |
15.5 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |