| Category | Polymer , Thermoplastic , Polyethylene (PE) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP STAT-KON |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics LNP STAT-KON FX98500C PE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.970 g/cc | 0.0350 lb/in³ | ISO 1183 |
| 0.976 g/cc | 0.0353 lb/in³ | ASTM D792 | |
| Moisture Absorption | 0.0200 % | 0.0200 % | 50% RH, 24 hrs; ASTM D570 |
| 0.0200 % | 0.0200 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.027 - 0.030 cm/cm @Time 86400 sec |
0.027 - 0.030 in/in @Time 24.0 hour |
ASTM D955 |
| 0.027 - 0.030 cm/cm @Time 86400 sec |
0.027 - 0.030 in/in @Time 24.0 hour |
ISO 294 | |
| Linear Mold Shrinkage, Transverse | 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ASTM D955 |
| 0.019 - 0.022 cm/cm @Time 86400 sec |
0.019 - 0.022 in/in @Time 24.0 hour |
ISO 294 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 13.0 MPa | 1890 psi | ASTM D638 |
| 14.0 MPa | 2030 psi | ISO 527 | |
| Tensile Strength, Yield | 23.0 MPa | 3340 psi | ASTM D638 |
| 23.0 MPa | 3340 psi | ISO 527 | |
| Elongation at Break | 43.2 % | 43.2 % | ASTM D638 |
| 82.8 % | 82.8 % | ISO 527 | |
| Elongation at Yield | 14 % | 14 % | ISO 527 |
| 15.8 % | 15.8 % | ASTM D638 | |
| Tensile Modulus | 0.870 GPa | 126 ksi | 1 mm/min; ISO 527 |
| 1.07 GPa | 155 ksi | 50 mm/min; ASTM D638 | |
| Flexural Strength | 26.0 MPa | 3770 psi | ASTM D790 |
| 27.0 MPa | 3920 psi | ISO 178 | |
| Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
| 0.930 GPa | 135 ksi | ISO 178 | |
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 21.0 J | 15.5 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| Impact Test | 63.0 J | 46.5 ft-lb | Multiaxial Impact; ISO 6603 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 48.0 °C | 118 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 46.0 °C @Thickness 3.20 mm |
115 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 100 ohm-cm - 1e+05 | 100 ohm-cm - 1e+05 | ASTM D257 |
| Surface Resistance | 100 ohm - 1e+05 | 100 ohm - 1e+05 | ASTM D257 |