Mechanical Properties Metric English Comments
Compressive Strength 98.1 MPa

@Temperature 1100 °C
14200 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 98.1 MPa

@Temperature 110 °C
14200 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics REFCAST LC90 Low Cement Castables
Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u..
Compressive Strength 98.1 MPa

@Temperature 1500 °C
14200 psi

@Temperature 2730 °F
Cold Crushing
Sharadaa Ceramics ZAP 002 Smart Cast Application
Special Properties: Thermal Shock Slag ResistanceIndustry: SteelApplication: Pig Iron Laddle working LayerInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 98.1 MPa

@Temperature 1100 °C
14200 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 003 Smart Cast Application
Special Properties: Anti-repellent PropertiesIndustry: CementApplication: Cement Plant Smoke ChamberInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 98.1 MPa

@Temperature 1100 °C
14200 psi

@Temperature 2010 °F
Cold Crushing
Sharadaa Ceramics ZAP 004 Smart Cast Application
Special Properties: Thermal Shock, Abrasion, Alkali ResistanceIndustry: SteelApplication: Lances, Launders, Riser TubesInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 98.1 MPa

@Temperature 110 °C
14200 psi

@Temperature 230 °F
Cold Crushing
Sharadaa Ceramics ZAP 007 Smart Cast Application
Special Properties: Hot abrasion, Wear resistanceIndustry: SteelApplication: False Chute, Tundish BackupInformation provided by Sharadaa Ceramics Pvt. Ltd.
Compressive Strength 98.1 MPa

@Temperature 1500 °C,
Time 10800 sec
14200 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories BLC Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1500 °C,
Time 10800 sec
14200 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CTL ARS Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1500 °C,
Time 10800 sec
14200 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 110 °C,
Time 86400 sec
14200 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1400 °C,
Time 10800 sec
14200 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-30KL Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1400 °C,
Time 10800 sec
14200 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-90 I Special SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1400 °C,
Time 10800 sec
14200 psi

@Temperature 2550 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-90S High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 1000 °C,
Time 10800 sec
14200 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SFC-90SC High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 98.1 MPa

@Temperature 110 °C,
Time 86400 sec
14200 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SFC-90W High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).