Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.011772 GPa

@Temperature 110 °C,
Time 86400 sec
1.7074 ksi

@Temperature 230 °F,
Time 24.0 hour
0.014715 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 ksi

@Temperature 2460 °F,
Time 3.00 hour
0.016677 GPa

@Temperature 1500 °C,
Time 10800 sec
2.4188 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 83.4 MPa

@Temperature 110 °C,
Time 86400 sec
12100 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
93.2 MPa

@Temperature 1350 °C,
Time 10800 sec
13500 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
98.1 MPa

@Temperature 1500 °C,
Time 10800 sec
14200 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1750 °C
3180 °F
limited
Shrinkage -0.190 %

@Temperature 1350 °C,
Time 10800 sec
-0.190 %

@Temperature 2460 °F,
Time 3.00 hour
-0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
1.0 %

@Temperature 1500 °C,
Time 10800 sec
1.0 %

@Temperature 2730 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 87 %
87 %
SiO2 7.0 %
7.0 %
Descriptive Properties Value Comments
Installation Method Casting, Vibrating
Material Required for Estimating(kg/?) 2,800
Water Required for Casting(%) 6.2