Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chosun Refractories SFC-90SC High-Alumina Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chosun Refractories SFC-90SC High-Alumina Castable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.016677 GPa
<br>@Temperature 110 °C,<br> Time 86400 sec
2.4188 ksi
<br>@Temperature 230 °F,<br> Time 24.0 hour
0.022563 GPa
<br>@Temperature 1000 °C,<br> Time 10800 sec
3.2725 ksi
<br>@Temperature 1830 °F,<br> Time 3.00 hour
0.023544 GPa
<br>@Temperature 1400 °C,<br> Time 10800 sec
3.4148 ksi
<br>@Temperature 2550 °F,<br> Time 3.00 hour
Compressive Strength 93.2 MPa
<br>@Temperature 110 °C,<br> Time 86400 sec
13500 psi
<br>@Temperature 230 °F,<br> Time 24.0 hour
Cold Crushing Strength
98.1 MPa
<br>@Temperature 1000 °C,<br> Time 10800 sec
14200 psi
<br>@Temperature 1830 °F,<br> Time 3.00 hour
Cold Crushing Strength
108 MPa
<br>@Temperature 1400 °C,<br> Time 10800 sec
15600 psi
<br>@Temperature 2550 °F,<br> Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1800 °C
3270 °F
limited
Shrinkage -0.350 %
<br>@Temperature 1400 °C,<br> Time 10800 sec
-0.350 %
<br>@Temperature 2550 °F,<br> Time 3.00 hour
-0.100 %
<br>@Temperature 1000 °C,<br> Time 10800 sec
-0.100 %
<br>@Temperature 1830 °F,<br> Time 3.00 hour
-0.0300 %
<br>@Temperature 110 °C,<br> Time 86400 sec
-0.0300 %
<br>@Temperature 230 °F,<br> Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 95 %
95 %
SiO2 4.0 %
4.0 %
Descriptive Properties Value Comments
Installation Method Self Flowing
Material Required for Estimating(kg/?) 3,100
Water Required for Casting(%) 5-5.5