Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST A High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C |
3560 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST Dense Castables Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST HA High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC60ABR Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC70 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics REFCAST LC90 Low Cement Castables Description: We bring to our clients a range of Low Cement Castables, that are available in varied alumina content and service range. Designed for abrasion resistance application, these are widely u.. |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C |
3560 psi @Temperature 230 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST LT Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST SPECIAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Compressive Strength | 24.5 MPa @Temperature 1400 °C |
3560 psi @Temperature 2550 °F |
Cold Crushing |
Sharadaa Ceramics Sharada AIO-SiC-C Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |
|||
Compressive Strength | 24.5 MPa @Time 86400 sec |
3560 psi @Time 24.0 hour |
Cold Crushing |
Sharadaa Ceramics ZAP 004 Smart Cast Application Special Properties: Thermal Shock, Abrasion, Alkali ResistanceIndustry: SteelApplication: Lances, Launders, Riser TubesInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Compressive Strength | 24.5 MPa @Temperature 1100 °C |
3560 psi @Temperature 2010 °F |
Cold Crushing |
Sharadaa Ceramics REFCAST C High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-C CM Conductive Polyimide Bearing Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-ESD CM Polyimide Bearing Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-N CM Unfilled Aromatic Polyimide Bearing Compression Molded. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS po.. |
|||
Compressive Strength | 24.5 MPa @Strain 1.00 % |
3550 psi @Strain 1.00 % |
ASTM D695 |
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi.. |
|||
Compressive Strength | 24.5 MPa @Temperature 500 °C, Time 10800 sec |
3560 psi @Temperature 932 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories APC-120G Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 1000 °C, Time 10800 sec |
3560 psi @Temperature 1830 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories BCT-145 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 29.4 MPa @Temperature 110 °C, Time 86400 sec |
3560 - 4270 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories HACT-180G High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTA-180 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTC-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 34.3 MPa @Temperature 1350 °C, Time 10800 sec |
3560 - 4980 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories PTF-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 110 °C, Time 86400 sec |
3560 psi @Temperature 230 °F, Time 24.0 hour |
Cold Crushing Strength |
Chosun Refractories FM Blast Furnace Runner Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 - 44.1 MPa @Temperature 1500 °C, Time 10800 sec |
3560 - 6400 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TPA-175 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 24.5 MPa @Temperature 1500 °C, Time 10800 sec |
3560 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TD-R75 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |