Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
|
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
|
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylene Sulfone (PPSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
|
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Very high dimensional stability. Good th.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 60.0 °C |
580 ksi @Temperature 140 °F |
|
LATI Latamid 12 H2 G/30 PA 12, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 90.0 °C |
580 ksi @Temperature 194 °F |
|
LATI Latamid 66 B G/20-V PA 66, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. High fluidity. Glass fibers. Flame retardant, non classifiable, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific;.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 150 °C |
580 ksi @Temperature 302 °F |
|
LATI Latamid 66 H2 G/25-V0KB PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 120 °C |
580 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 G/25-V0KB1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 150 °C |
580 ksi @Temperature 302 °F |
|
LATI Latamid SP2 H2 G/45 PA 6.12, 45% Glass Fiber Reinforced, Heat Stabilized Polyamide 6.12 (PA6.12) based compound. Heat stabilized. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provi.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 90.0 °C |
580 ksi @Temperature 194 °F |
|
LATI Latan 13 G/30 POM, 30% Glass Fiber Reinforced Polyoxymethylene (POM) based compound. Glass fibers. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation .. |
|||
Tensile Modulus | 4.00 GPa @Temperature 150 °C |
580 ksi @Temperature 302 °F |
|
LATI Latigloss 57 G/40 F2 PPA, 40% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact applicationAvailability: Af.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 150 °C |
580 ksi @Temperature 302 °F |
|
LATI Latigloss 66 H2 G/50 F2 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Potentially suitable for food/medical contact application. Availab.. |
|||
Tensile Modulus | 4.00 GPa @Temperature 23.0 °C |
580 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |