Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.50 GPa @Thickness 0.100 mm |
508 ksi @Thickness 0.00394 in |
MD; ISO 527 |
Victrex® APTIV® 2102-100M Polyetheretherketone (PEEK) Polymer Film, Amorphous, Mineral Filled APTIV® 2100 series films are the mineral filled amorphous films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications. APTIV .. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 60.0 °C |
508 ksi @Temperature 140 °F |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
|
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 G/25-V0HF1 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good mechanical properties. Very good electrica.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 150 °C |
508 ksi @Temperature 302 °F |
|
LATI Latamid 66 H2PX-V2 PA 66, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Toughened. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin A.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Latamid 66 VH G/30 PA 66, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Hydrolysis stabilized. Glycol stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Latamid 66 H2 G/25-V0KB3 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaIn.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Later 4E61 GCER/450-V0 PBT, Glass/Mineral Filled, Flame Retardant Polybutylene Terephthalate (PBT) based compound. Toughened. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very good electrical properties.Avail.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 120 °C |
508 ksi @Temperature 248 °F |
|
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Tensile Modulus | 3.50 GPa @Temperature 23.0 °C |
508 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® BM70G15HSLR BK537 Nylon 66 Zytel® BM70G15HSLR BK537 is a 15% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers |