Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.75 kN/m | 10.0 pli | 1 oz. Cu, after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Peel Strength | 1.75 - 2.10 kN/m | 10.0 - 12.0 pli | |
ITW Devcon Plastic Welderâ„¢ Methacrylate Adhesive SD, Off-White Information provided by ITW Devcon |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al/Al |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel |
Master Bond EP76M-1R Nickel Conductive Epoxy Adhesive Description: Master Bond Polymer System EP76M-1R is a two component, nickel filled, electrically conductive adhesive for high performance bonding formulated to cure at room temperature or more rapid.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | |
Master Bond EP79 Two Component, Silver Coated, Nickel Filled Conductive Epoxy Master Bond Polymer System EP79 is a two component, silver coated, nickel filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or .. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al to Al |
Master Bond Supreme 46HT-2 Toughened, High Shear and Peel Strength Adhesive Description: Master Bond Supreme 46HT-2 is a two component epoxy adhesive featuring an attractive balance of good shear and peel strengths for high performance structural bonding and coating suitabl.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | Bond Strength |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Bond Strength; ASTM D624 |
Arlon P29514R015 0.0165" (0.419 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Self-Fusing Silicone RubberSubstrate: 7727 Style FiberglassProduct Advatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under loa.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to Steel; ASTM D1000 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | on canvas |
3M Scotch-Weld™ 3797 Hot Melt Adhesive High ball and ring; Low viscosity and Good for electrical pottingInformation provided by 3M |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Faceside, to Stainless Steel, 180° Peel, 2 mil Al |
3M XP2112 Hi-Performance Adhesive Transfer Tape 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | (S1 to S1), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | 90° Peel, PET/Stainless Steel, 72 hrs at 70°C; ASTM D3330 |
3M 7953MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Polypropylene, 180°, 2 mil al foil, 30 sec RT, Faceside; ASTM D3330 |
3M 9627 Adhesive Transfer Tape with Quick Bonding Adhesive 360 3M™ Adhesive Transfer Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated pai.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to PVC |
3M EPS-200 Tubing 3M EPS-200 is a 2:1 thin-wall tubing offering the advantages of integral adhesive-lined construction. The tubing is made from a flame-retardant, flexible polyolefin with a thing layer of special the.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Adhesion to PVC |
3M EPS-300 Heat Shrink Tubing 3M Heat Shrink tubing EPS-300 is a 3:1 thin-wall, flexible tubing offering the advantages of integral, adhesive-lined construction. The tubing is made from flame-retardant, flexible polyolefin with .. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | T-Peel |
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Stainless Steel 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | ABS, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Polycarbonate, 180°, 2 mil al foil, 72 hr RT, Backside; ASTM D3330 |
3M 9629PC Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | T-Peel |
3M Scotch-Weld™ 1386 One-Part Epoxy Adhesives and Metal Primer High Temperature strength and Impact resistanceInformation provided by 3M |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | T-Peel; ASTM D1876 |
3M Scotch-Weld™ 2290 Epoxy Adhesive/Coating 3M™ Scotch-Weld™ Epoxy Adhesive/Coating 2290 is an amber tinted thermo-setting adhesive/coating for metal to metal bonding and coating. It can be used to assemble laminated steel cores for electri.. |
|||
Peel Strength | 1.75 kN/m | 10.0 pli | Steel T-Peel; ASTM D1876 |
3M Scotch-Weld™ DP 3501 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi.. |
|||
Peel Strength | >= 1.75 kN/m | >= 10.0 pli | T-peel, Al to Al |
Master Bond Supreme 3AN One Component, Heat Curing Epoxy Adhesive Description: Master Bond Polymer System SUPREME 3AN is a one component, heat cured epoxy adhesive and sealant, featuring high peel and shear strength along with excellent thermal conductivity and co.. |