Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.175 - 14.4 kN/m | 1.00 - 82.0 pli | Average value: 4.88 kN/m Grade Count:144 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Peel Strength | 0.175 - 0.1972 kN/m | 1.00 - 1.125 pli | Adhesion |
Dielectric Polymers NT-500 Protective Film
(discontinued **) Crosslinked silicone adhesive with electrical grade polyester film backing.Features: Clean tape removalNo film shrinkage after exposure to elevated temperaturesApplications: Used as a fume mask duri.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Steel; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Backing; ASTM D1000 |
3M 1400 Economy Vinyl Electrical Tape 3M™ Economy Vinyl Electrical Tape 1400 is a black 7 mil thick, general use vinyl-insulating tape. It is designed to perform continuously in temperatures up to 80°C. This tape has a polyvinyl chlor.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7840TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Materials 7840 and 7840TL are matte radiant white polyester label stocks that offer . These label products utilize 3M™ Adhesive 310 which is a firm adhesi.. |
|||
Peel Strength | >= 0.175 kN/m | >= 1.00 pli | to Arlon 51270R015, Bond Strength; Arlon SQA -TMS-011 |
Arlon 680-R3839R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Peel Strength | >= 0.175 kN/m | >= 1.00 pli | to Arlon 51270R015, Bond Strength; Arlon SQA -TMS-011 |
Arlon 680-R3844R 0.084" (2.13 mm) Cured Silicone Coating with Silica-based Substrate Design/Construction:Side 1: Cured Silicone Coating Substrate: Silica-basedSide 2: Cured Silicone Coating Rubber Application Advantages:Extremely low thermal conductivityThermally stableBondable to s.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Tape Property; MIL-I-46852C |
Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner Description: 1 inch wide, 50 mil thick, Red, Rectangular cross-section, Fully cured silicone interleaved with 0.002” PSA liner. Product is supplied in various roll lengths and the xx in the product.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Steel; ASTM D3330 |
3M Highland™ 5910 Transparent Tape Scotch® Tape 5910 is a utility grade transparent tape designed for light-duty packaging applications, that is typically used for bag closing, temporary holding, and L-clip applications that do not .. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 8004 Specialty Performance Film Tape Scotch® Specialty Performance Film Tape 8004 is designed for lifting and preserving physical evidence such as finer prints. This ultra clean tape is resistant to moisture and resists degradation du.. |
|||
Peel Strength | 0.175 - 0.351 kN/m | 1.00 - 2.00 pli | T-Peel |
3M Scotch-Weld™ CA5 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Higher viscosity, slower setting version of CA4 for filling gaps. Meets CID A-A-3097, Type II, Clas.. |
|||
Peel Strength | 0.175 - 0.351 kN/m | 1.00 - 2.00 pli | T-Peel |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | |
3M Scotch-Weld™ DP100 Plus Clear Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP100 Plus Clear is a fast setting, two-part, 1:1 mix ratio mercaptan-cured epoxy adhesive. It is a unique among fast setting mercaptan cure epoxies in that it comb.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | 180°, Glass |
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | HD Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7011FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Polyethylene; ASTM D3330 |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ IJ160 Graphic Film 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |
|||
Peel Strength | 0.175 - 0.351 kN/m | 1.00 - 2.00 pli | T-Peel |
3M Scotch-Weld™ CA40 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to many substrates including flexible vinyl and EPDM rubbe.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | 180° |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | 180°, Polystyrene |
3M Scotch-Weld™ TS115 HGS Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Peel Strength | 0.175 kN/m | 1.00 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7897 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 310 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.175 - 0.351 kN/m | 1.00 - 2.00 pli | T-Peel; ASTM D1876-61T |
3M Scotch-Weld™ CA4 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M |
|||
Peel Strength | 0.175 - 0.877 kN/m | 1.00 - 5.00 pli | Varies with substrates. |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Peel Strength | 0.175 - 0.877 kN/m | 1.00 - 5.00 pli | Varies with substrates. |
Loctite® Durabond® E-00NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Peel Strength | 0.175 - 0.877 kN/m | 1.00 - 5.00 pli | Varies with substrates. |
Loctite® Durabond® E-60NC Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |