Dielectric Polymers NT-500 Protective Film  (discontinued **)

Category Polymer , Adhesive , Film , Thermoset , Polyester, TS , Silicone
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dielectric Polymers NT-500 Protective Film  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Crosslinked silicone adhesive with electrical grade polyester film backing.Features: Clean tape removalNo film shrinkage after exposure to elevated temperaturesApplications: Used as a fume mask during plating and to protect a variety of substrates during fabrication, installation, shipping and storage.Information provided by Dielectric Polymers.
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Adhesive
127 microns
5.00 mil
Backing
Mechanical Properties Metric English Comments
Elongation at Break 150 %
150 %
Peel Strength 0.175 - 0.1972 kN/m
1.00 - 1.125 pli
Adhesion
26.3 kN/m
150 pli
Tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
>= 260 °C
>= 500 °F
Shear Adhesive Failure (polyester failure)
Descriptive Properties Value Comments
Color White