Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Plaskolite PETG Mirror Sheet Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® MC8100 PC+ABS (Asia Pacific) Extrusion blowmolding grade. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy EXGY30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy FXTW30CP ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
LG Chemical HI-151 ABS, Middle Impact Information Provided by LG Chem |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Europe-Africa-Middle East) LNP* LUBRICOMP* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features include Internally Lubricated. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP GL003XXP PSU (Europe-Africa-Middle East) LNP* LUBRICOMP* GL003XXP is a compound based on Polysulfone resin containing PTFE. Added features include; Internally Lubricated. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® HX3091HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® 1103 PBT+PC AUTOMOTIVE. Unreinforced, impact modified PBT+PC alloy. Excellent low temperature impact and chemical resistance. Range gray, black colors. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ASTM D790 |
Wanshijie PETG Sheet PETG is also named GPET. It is made of a kind of non-crystalline PET resin sourced from cyclohexanediol modification. PETG differs greatly from PET and PCT. PETG is a kind of non-crystalline copolym.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | ISO 178 |
Eastman Eastar EN001 Copolyester Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming pro.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ASTM D790 |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Asia Pacific) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Noryl FXN119LG PPE+HIPS (Europe-Africa-Middle East) Noryl FXN119LG is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119LG is available in mutliple colors.This da.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Asia Pacific) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0712 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0712 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 37% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 77.0 MPa | 11200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics XYLEX FXY330DF PC+POLYESTER (Asia Pacific) Polyester+PC alloy. Diffusion Effect. Color package may affect performance. |