Mechanical Properties Metric English Comments
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM D790
Nylene® 603 Nylon 6, Extrusion Grade
Dry as molded. Extrusion grade. Nylene 603 is a plasticized, high residual monomer resin designed for extrusion applications requiring excellent flexibility, high strength and good abrasion resist..
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycolac® MG34LGHF ABS
Low gloss, high flow ABS for unpainted interior applications.This data was supplied by SABIC-IP for the Americas region.
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM D790
Ineos Nova 2100 General Purpose Crystal Polystyrene  (discontinued **)
Relative high heat resistance, Improved crack resistance, Good strengthApplications: Foam extrusion, Biaxially oriented sheet, Thermoforming applications, Molded packagingExposure to gamma radiation..
Flexural Yield Strength 61.0 - 83.2 MPa
8850 - 12100 psi
Average value: 74.2 MPa Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM-D790
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
Flexural Yield Strength 61.0 MPa

@Strain 3.50 %
8850 psi

@Strain 3.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66
PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Yield Strength 61.0 MPa
8850 psi
at 5% strain; ASTM D790
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned
Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with
Flexural Yield Strength 61.0 MPa
8850 psi
at 5% strain; ASTM D790
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned
Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi..
Flexural Yield Strength 61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11
LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer containing PTFE / Silicone. Added features include: Inernally Lubricated
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP KP004AXP POM (Europe-Africa-Middle East)
LNP* LUBRICOMP* KP004AXP is a compound based on Acetal Homopolymer containing PTFE, Silicone. Added features include Internally Lubricated.
Flexural Yield Strength 61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP
LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant...
Flexural Yield Strength 61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Flexural Yield Strength 61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WP004 is a compound based on Polybutylene Terephalate resin containing PTFE, Silicone. Added features include ; Internally Lubricated.
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Flexural Yield Strength 61.0 MPa
8850 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11
LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity.
Flexural Yield Strength 61.0 MPa
8850 psi
ASTM D790
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded
Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar.
Flexural Yield Strength 61.0 MPa
8850 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermotuf P1000IX3 PA 6 (Europe-Africa-Middle East)
LNP* THERMOTUF* P1000IX3 is a compound based on PA6 resin containing Impact Modifier. Added features include : High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
Flexural Yield Strength 61.0 MPa
8850 psi
6.4 mm; ASTM D790
SABIC Innovative Plastics NORYL FN215X PPE+PS
Structural foam resin. 170F (77C) HDT. Improved reliability and productivity. All values at 20% weight reduction.