Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Flexural Yield Strength | 179 - 432 MPa | 26000 - 62700 psi | Average value: 295 MPa Grade Count:18 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES Electrablend® PC CF20 CR X 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Good Chemical Resistance and Semi ConductiveInformation provided by TP Compos.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES Electrablend® PC CF20 FR IM BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Frame Retardant, Impact Modified and Semi Conductive.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES Electrablend® PC/PET CF20 IM 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact Modified and Semi ConductiveAppearance: Black.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES HiFill® PP LGF50 CC NAT 12mm 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Long Glass Fiber, 50% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF006RXQ PC LNP* THERMOCOMP* DF006RXQ is a compound based on Polycarbonate resin containing 30% Glass Fiber. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF008 Acetal Copolymer (Europe-Africa-Middle East) LNP* THERMOCOMP* KF008 is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Clariant Renol 612G20-L Nylon 612, 20% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Ascend Performance Materials VYDYNE® R513 Nylon, 13% Glass Reinforced Typical property data. VYDYNE is a registered trademark of Solutia Inc. |
|||
Flexural Yield Strength | 179 - 221 MPa | 26000 - 32000 psi | Average value: 200 MPa Grade Count:10 |
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated. |
|||
Flexural Yield Strength | 179 MPa | 26000 psi | ASTM D790 |
Techmer ES HiFill® PP LGF40 CC HS BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled and Heat StabilizedAppearance: Bla.. |